Abstract
High temperature tensile tests have been conducted on samples of a Fe-Ni based superalloy, Incoloy A-286, and significant ductility loss has been observed at 1220 °C. Titanium-rich, thin-film-like phase has been found on the inter-granular facets of fracture surfaces. It appears that sulfur content of Ti-rich phase was higher than that of the matrix. At 1220 °C, liquation of Ti-rich phases has resulted in thin-film-like morphology along the grain boundary and caused the ductility loss during tensile deformation.
Abstract licence: CC BY
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.