The Mechanical Properties of the Extra Hard Spring Arch Wire Subjected to the Artificial Saliva
Hussain A Obaidi, Sarmad S Al–Qassar
Al-Rafidain Dental Journal · 2009
doi:10.33899/rden.2009.9005 (opens in a new tab)
We email you when a new notice or a question about this paper appears.
Abstract
Aims: To evaluate and compare the value of the mechanical properties of the extra hard spring stainlesssteel arch wire immersed in artificial saliva. Materials and Methods: The sample consisted of 40extra hard spring stainless steel arch wires (Remanium, 0.016″ × 0.016″, Dentarum, Germany) dividedinto; control wires group and experimental group (ten wires for each group). The experimental groupwas immersed in artificial saliva (PH 6.75+ 0.015) ) and incubated at 37 for one, two and four weeksrespectively. The curve of tensile strength for the control and experimental groups was performed usingthe tensile testing machine. The mechanical properties of the arch wire have been derived. The resultswere analyzed using the statistics of descriptive, Anova and Duncan’s Multiple Range Analysistests. Results: The results showed that the mechanical properties (ultimate tensile strength, elasticmodulus, springiness (springback),elastic limit, plastic limit (ductility) of the extra spring hard stainlesssteel arch wire significantly decrease as the immersion time in artificial saliva increase when comparedwith the control group. Conclusions: It is recommended not utilize the extra spring hard stainlesssteel arch wire for long periods during orthodontic treatments.
Abstract licence: CC BY
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.