Fabrication and Optimization of Electrophoretic Deposition Parameters Using Alternating Current by Taguchi Design
Muna Khethier Abbass, Mohammed Jasim Khadhim, Ayad Naseef Jasim and 2 more
مجلة النهرين للعلوم الهندسية · 2021
doi:10.29194/njes.24010008 (opens in a new tab)
We email you when a new notice or a question about this paper appears.
Abstract
The aim of this work is to optimize EPD variables (voltage, time, and focus) using alternating current through the Taguchi Design of Experiment (DOE). Coating Nano hydroxyapatite (Nano-HA) on a Ti6Al4V substrate depends on thickness and roughness, then characterization of a coating layer to determine the optimum state. Hydroxyapatite (HAp) powder was deposited on a Ti-6Al-4V alloy substrate by electro-deposition with ethanol as a solvent under AC current, to improve the alloy surface quality based on coating thickness and maximum coating mass meeting the requirements of a biological orthopedics application. Ethanol was used as a solvent to precipitate ketazone and HAp on the base alloy. Taguchi's approach was used in order to determine the optimal conditions for EPD and subsequently to apply various criteria for depositing the biochemical coating. The surface and cross-section composition of the paint is described by characterization. Numerous tests and inspections; Zeta, XRD and SEM stability test, water contact angle and optical microscopes were used to describe the surface morphology of the HAp layer. The value of the optimum conditions for deposition of the HAp layer which is a simultaneous thickness and maximum coating mass, was predicted at a sedimentation voltage of 40 V, 2 min sedimentation time and 1 g / L for the concentration of the suspended solution at room temperature. The validity of the model resulting from the response surface methodology was assessed by comparing the expected results with the experimental results. In addition, close agreement was observed between the experimental results and the expected results. For the solution at room temperature, the results obtained with the highest value of the coating thickness of 41at the surface roughness of 0.94 and the contact angle of the alloy before coating is 67.489º reduced to. 38.132º after plating, which indicates an increase in the harmony of the metal implant and biocompatibility.
Abstract licence: CC BY-NC
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.