Preparation of titanium carbide powder from ilmenite concentrate
Gou Hai-Peng, Zhang Guo-Hua, Kuo-Chih Chou
Chemical Industry and Chemical Engineering Quarterly · 2017
doi:10.2298/ciceq150521007g (opens in a new tab)
We email you when a new notice or a question about this paper appears.
Abstract
A new process of producing titanium carbide powder from ilmenite concentrate was put forward. The ilmenite concentrate was reduced by graphite powder at 1500ºC for 6 hours, with the reduction products of TiC, Fe and MgO. The porous reduction products were agitation leached in ferric chloride solution at 25ºC for 60 minutes. After the filtration, TiC powder accompanied by little MgAl2O4 and Mg2SiO4 were obtained. Finally, the element Fe was recycled from the filtrate in the form of β-FeOOH after blowing air for 3 hours at 80ºC. The size of rod-like β-FeOOH particle was less than 1µm.
Abstract licence: CC BY
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.