The effect of steaming time and resin content on MDF made from canola straw
Hossein Usefi, Ali akbar Enayati, Mohammad mehdi Faezi poor and 1 more
تحقیقات علوم چوب و کاغذ ایران · 2008
doi:10.22092/ijwpr.2008.117412 (opens in a new tab)
We email you when a new notice or a question about this paper appears.
Abstract
Canola straw as a agricultural residues has been investigated for MDF production. The variables were the steaming time of 2, 5 & 8 minutes and the resin content of 9 and 11 present. Other factors being kept constant. Some of the physical and mechanical properties such as thickness swelling (TS), water absorption (WA) modulus of rupture (MOR), modulus of elasticity (MOE), internal bond (IB), were measured. In addition, canola straw fiber properties such as fiber length, diameter and cell wall thickness were determined. The results showed that the optimum condition for MDF production from canola straw is the treatment of 5 minutes steaming time and 11% resin content. All the tested mechanical and thickness swelling properties improved with the increase of steaming time level. Dimensional stability of the MDFs improved as resin content increased. WA and TS values of the produced boards were relatively high because no wax and no depithing were used during the board production. More over, the values of canola straw fiber length, diameter and cell wall thickness are 1215, 28, 7.43 micrometer respectively.
Abstract licence: CC BY
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.