Estimation of pyrolysis product of LDPE degradation using different process parameters in a stirred reactor
Mehrdad Seifali Abbas-Abadi, Mehdi Nekoomanesh Haghighi, Armando G. McDonald and 1 more
Polyolefins Journal · 2015
doi:10.22063/poj.2015.1102 (opens in a new tab)
We email you when a new notice or a question about this paper appears.
Abstract
Pyrolysis of low density polyethylene (LDPE) by equilibrium fluid catalytic cracking (FCC) was studied in a stirred reactor under different process parameters. In this work, the effect of process parameters such as degradation temperature (420-510°C), catalyst/polymer ratio (0-60%), carrier gas type (H2, N2, ethylene, propylene, Ar and He), residence time and agitator speed (0-300 rpm) on the condensate yield (liquid, gas and coke) and product composition were considered. Reaction products were determined by GC analysis and shown to contain naphthenes (cycloalkanes), paraffins (alkanes), olefins (alkenes) and aromatics. Higher temperature and more catalyst amount enhanced LDPE cracking. The maximum “fuel like” condensed product yield was attained at 450°C and 10% catalyst, respectively and gaseous products increased with increases in temperature. Hydrogen as a reactive carrier gas increased the condensed and paraffinic product yield. Appropriate heat transfer (by stirring) increased the catalyst efficiency in a stirred reactor.
Abstract licence: CC BY-NC-SA
References32
32 more references, whose wording the paper’s licence keeps private.
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.