A Study on the Recovery of Titanium Dioxide from a Blast Furnace Slag, Using Roasting and Acid Leaching
mohsen fattahpour, Mohammad Noaparast, Ziaedine Shafaei and 2 more
International Journal of Mining and Geo-Engineering · 2019
doi:10.22059/ijmge.2018.264394.594756 (opens in a new tab)
We email you when a new notice or a question about this paper appears.
Abstract
In this research, parameters affecting the recovery of titanium dioxide from Iron slag sample collected from Esfahan Steel Company, located in Esfahan province, Iran, were studied. Roasting with sodium carbonate followed by sulfuric acid leaching was used in this study. The best condition for roasting with sodium carbonate was obtained at the temperature of 500oC with Na2CO3/slag ratio of 1/4, and in 120 minutes. The optimum condition for titanium dioxide recovery from iron blast furnace slag was achieved at temperature of 85oC, Solid/Liquid ratio of 1/15, sulfuric acid concentration of 2 M in 240 minutes time, for -106µm sized sample. The maximum recovery was 53%. The kinetic study showed that the leaching process was controlled by the diffusion, in which the activation energy was 5.85kJ/mol which confirmed the diffusion control of the process.
Abstract licence: CC BY
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.