PENGAWETAN LIMA JENIS KAYU MENURUT METODE RENDAMAN PANAS-DINGIN
Barly Barly, Pipin Permadi
Jurnal Penelitian Hasil Hutan (Journal of Forest Products Research) · 2017
doi:10.20886/jphh.1988.5.5.265-268 (opens in a new tab)
We email you when a new notice or a question about this paper appears.
Abstract
The degree of protection offerd by a wood preservative depends upon the quality of preservative retained by the timber, the depth penetration, and the permanence of preservative in the wood. On the hot and cold bath process, the timber is immersed in cold preservative and the bath and timber are heated up together to around 70°C for one, two, three hours until the timber is hot throught, and the whole then allowed to cool down for 24 hours. For all timber species tested in this experiment the depth of penetration and retention of preservative was measured after treatment. The result of which can be seen in Table 1. After calculated and analysis (Table 2 and Table 3) the following conclusions could be draw: • Timber species has highly significant on boron penetration and retention. Boron penetration a seemed to be generally getting deeper with increased hot soaking hours; but one hour is fully. • Generally speaking, hot and cold bath process are to be preferred although with mahoni (Swietenia mahogani Jack:) and tanjung (Mimmusops elengi L.) timbers the preservative retention less than the other timbers.
Abstract licence: CC BY-NC-SA
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.