The Study aimed at improving the quality of chrome-tanned leather for golf floves producted by Indonesian tanners. Samples used in this study were 32. They were visually inspected and tested on their chemical and physical properties. The results of the chemical and physical tests were analyzed using deviation standard in descriptive statistics. It was obtained from the visual inspection of the samples taken that the leather was soft enough, the colour was even, their hair was not loose, and it was flexible but not elastic. While from the Chemical Tests, the results obtained were: water content (13,78 – 16,94) %; Fat Content (6,04 – 11,38) % and pH Valueness (4,43 – 5,19). It was obtained from the physical tests that Thickness (0,32 – 0,64) mm; well tanned; Tensile Strength resistence (106,07 – 109,73) kg/cm2; Flexibility (53,11 – 103,07) %; Slit Tear Resistance (13,48 – 39,22) kgf/cm; Stitch Tear Strength (74,51 – 137,79) kgf/cm, wet rub fastness tst shown a little discolourisation while dry rub fastness test shown no discolourisation.
Abstract licence: CC BY
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.