Dimensional change of acrylic resin plate after the reinforcement of glass fibre
Dwiyanti Feriana Ratwita, Rinda Mahalistiyani
Dental Journal · 2007
doi:10.20473/j.djmkg.v40.i2.p61-64 (opens in a new tab)
We email you when a new notice or a question about this paper appears.
Abstract
<span style="font-family: Tribune-Italic; font-size: 9pt; color: #231f20; font-style: normal; font-variant: normal;"><em>The effect of fibre reinforcement of polymethyl methacrylate was investigated. Glass fibres have been studied as strengthening </em><span style="font-family: Tribune-Italic; font-size: 9pt; color: #231f20; font-style: normal; font-variant: normal;"><em>material added to polymethyl methacrylate. The purpose of this study was to evaluate dimensional change of acrylic resin plate after </em><span style="font-family: Tribune-Italic; font-size: 9pt; color: #231f20; font-style: normal; font-variant: normal;"><em>glass fibre reinforcement. As a research subject is an acrylic resin plate of 65 </em><span style="font-size: 10pt; color: #231f20; font-style: normal; font-variant: normal;"><em>× </em><span style="font-family: Tribune-Italic; font-size: 9pt; color: #231f20; font-style: normal; font-variant: normal;"><em>10 </em><span style="font-size: 10pt; color: #231f20; font-style: normal; font-variant: normal;"><em>× </em><span style="font-family: Tribune-Italic; font-size: 9pt; color: #231f20; font-style: normal; font-variant: normal;"><em>2.5 mm with the number of 32 samples were </em><span style="font-family: Tribune-Italic; font-size: 9pt; color: #231f20; font-style: normal; font-variant: normal;"><em>distributed randomly in 4 experimental groups. Each group consisted of 8 samples and control groups. Group 1: acrylic resin plate </em><span style="font-family: Tribune-Italic; font-size: 9pt; color: #231f20; font-style: normal; font-variant: normal;"><em>and 1 sheet glass fibre; group 2: acrylic resin plate and 2 sheet glass fibre; group 3: acrylic resin plate and 3 sheet glass fibre. Control </em><span style="font-family: Tribune-Italic; font-size: 9pt; color: #231f20; font-style: normal; font-variant: normal;"><em>group which was not given treatment. Dimensional change was measured by profile projector. The data was analyzed by One-Way </em><span style="font-family: Tribune-Italic; font-size: 9pt; color: #231f20; font-style: normal; font-variant: normal;"><em>ANOVA and LSD test showed that there was significant difference in dimensional change (p < 0.005). The conclusion suggested that </em><span style="font-family: Tribune-Italic; font-size: 9pt; color: #231f20; font-style: normal; font-variant: normal;"><em>dimensional change of the acrylic resin plates after glass fibre reinforcement minimally done 1 sheet glass fibre.</em></span></span></span></span></span></span></span></span></span></span></span></span>
Abstract licence: CC BY-SA
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.