Abstract
The research of smelting low ferronickel from pre-concentrate nickel-iron ore with 2.76 % Ni and 38.00 % Fetotal was carried out to find an effective way for stainless steel enterprises to use the low-nickel laterite reasonable. The results show that Ni and Fe both have a certain degree of enrichment, and impurities and harm elements have different degrees of reduction after pre-concentration of nickel-iron ore. Most valuable metal did not compound with impurities which greatly accelerated the speed and extent of melt separation reduction. Good alloy of 6.58 % Ni with the overall recoveries of 93.38 % and 89.95 % Fetotal with the overall recoveries of 89.57 % was manufactured under the following conditions: 10 % coke, 1.0 binary basicity, 18 % MgO and 3 % Al2O3 in slag, melting at 1,550 °C for 10 min. The product can be used for the feed of producing stainless steel.
Abstract licence: CC BY
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.