Abstract
In the present study, mechanical properties of 0.25Li2O.2SiO2-0.75BaO.2SiO2 glass-ceramic were investigated. The trans-formations‘ temperatures were determined by DTA instrument. The optimum nucleation temperature was found to be 540°C. This suggested the crystallization temperatures as 675, 720 and 800°C. After carrying out crystallization heat treatments, Vickers indentation test was applied. In order to determine the indentation fracture toughness (KIC), crack half-length ‚c‘ of the samples was measured. To calculate KIC, Young’s modulus, E and the measured hardness, Hv were used. Using KIC and probability of fracture ‚P‘, ln ln[1/(1 − P)] – ln KIC graph was drawn based on the Weibull distribution equation. Consequently, Weibull modulus, ‚m‘ and scale parameter, ‚K0‘ were determined and compared with each other.
Abstract licence: CC BY
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.