High Temperature Deformation Flow Of A ZK60A Magnesium Alloy After Extrusion

Kawasaki M., Lee H.-J., Oh M.C. and 1 more

Archives of Metallurgy and Materials · 2015

doi:10.1515/amm-2015-0124 (opens in a new tab)

We email you when a new notice or a question about this paper appears.

Abstract

Flow behavior of a ZK60A magnesium alloy after continuous casting and subsequent extrusion was examined in tension at a range of strain rates of 3.0×10−6 − 1.0×10−2 s−1 at temperatures of 473-623K. The results demonstrated that the alloy exhibited a maximum elongation of ~250% at 523K when tested at an initial strain rate of 1.0×10−5 s−1 and strain rate sensitivity, m, of ~0.3-0.4 and the activation energy of ~94 kJ/mol were calculated under the testing conditions. The detailed investigation suggested that the high temperature flow of the ZK60A alloy having submicrometer grains demonstrates quasi-superplastic flow behavior controlled by a dislocation viscous glide process.

Abstract licence: CC BY

Reads

Read by people on this page

None yet.

Checked or read by AI through naulon

None yet.

A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.

Are you an author?

Is this your paper?

Claim it to add your note and be paid when agents cite it. Free.