Cathodoluminescence Study of Damage Formation and Recovery in Si-ion-implanted β-Ga 2 O 3

Ryuichi Sugie, Tomoyuki Uchida, Ai Hashimoto and 3 more

IEEE Journal of the Electron Devices Society · 2022

doi:10.1109/jeds.2021.3134407 (opens in a new tab)

We email you when a new notice or a question about this paper appears.

Abstract

Ion implantation and activation annealing are key processes in the creation of an ideal free carrier distribution in semiconductor devices. Ultra-wide-bandgap (UWBG) semiconductors, such as gallium oxide (Ga<sub>2</sub>O<sub>3</sub>) and aluminum nitride (AlN), have many advantages suitable for power-device applications. We implanted silicon (Si) at doses ranging from <inline-formula> <tex-math notation="LaTeX">$1 \times 10^{11}$ </tex-math></inline-formula> to <inline-formula> <tex-math notation="LaTeX">$1 \times 10^{15} \mathrm{~cm}^{-2}$ </tex-math></inline-formula> into <inline-formula> <tex-math notation="LaTeX">$\beta-\mathrm{Ga}_2 \mathrm{O}_3$ </tex-math></inline-formula> (&#x2212;201) wafers, and annealed them at 800 and 1000&#x00B0; C in N<sub>2</sub> atmosphere. Secondary ion mass spectrometry (SIMS) and cathodoluminescence (CL) were used to evaluate the dopant profile and damage resulting from ion implantation. The CL intensity decreased rapidly with the dose. Even at a dose of <inline-formula> <tex-math notation="LaTeX">$1 \times 10^{11} \mathrm{~cm}^{-2}$ </tex-math></inline-formula>, the intensity dropped by nearly half of its value for the bare wafer. The CL intensity recovered after annealing at all doses; however, the CL intensity did not fully recover even after annealing at 1000&#x00B0;C. Moreover, the CL-depth profile at a dose of <inline-formula> <tex-math notation="LaTeX">$1 \times 10^{15} \mathrm{~cm}^{-2}$ </tex-math></inline-formula> after annealing at 1000&#x00B0;C showed pronounced intensity decay near the Si-diffused region. The CL-intensity decay was strongly correlated with Si diffusion. This phenomenon suggests that high-temperature annealing at high dose not only activates the Si dopant through the interaction of the interstitial Si and Ga vacancies but also causes interstitial Si atoms to diffuse into deeper regions. CL spectroscopy is very sensitive to the implantation damage and can be used for optimization of ion implantation and annealing processes in <inline-formula> <tex-math notation="LaTeX">$\beta_{-\mathrm{Ga}_2 \mathrm{O}_3}$ </tex-math></inline-formula>.

Abstract licence: CC BY-NC-ND

References38

    38 more references, whose wording the paper’s licence keeps private.

    Reads

    Read by people on this page

    None yet.

    Checked or read by AI through naulon

    None yet.

    A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.

    Are you an author?

    Is this your paper?

    Claim it to add your note and be paid when agents cite it. Free.