Mechanical properties and tribological characteristics of B4C-SiC ceramic composite in artificial seawater

Wei Chen, Hao Wenhui, ziqiang Zhao and 3 more

Journal of Asian Ceramic Societies · 2021

doi:10.1080/21870764.2021.1986202 (opens in a new tab)

We email you when a new notice or a question about this paper appears.

Abstract

To improve the mechanical properties and tribological characteristics of boron carbide (B4C) ceramic, silicon carbide (SiC) as an incorporation phase was added into boron carbide matrix. The results showed that, the incorporation of SiC phase led to denser microstructure and lower porosity. When SiC content was 20 wt.%, the bending strength and fracture toughness of the ceramic composite were 447.6MPa and 7.21 MPa·m1/2, respectively. Under seawater lubrication, the friction coefficient of B4C-20%SiC was lowered to 0.052, and the wear rate of ceramic composite was lower than the magnitude of 10−6mm3/Nm. The excellent tribological performance was attributed to lubricating, cooling of seawater, and tribochemical reaction.

Abstract licence: CC BY-NC

Reads

Read by people on this page

None yet.

Checked or read by AI through naulon

None yet.

A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.

Are you an author?

Is this your paper?

Claim it to add your note and be paid when agents cite it. Free.