Abstract

Realization of heterostructures containing multiple two-dimensional electron liquids requires a fine control of the fabrication process. Here, we report a structural and spectroscopy study of LaAlO3/SrTiO3/LaAlO3 trilayers grown on the SrTiO3 substrate by pulsed-laser deposition. Scanning transmission electron microscopy with the help of ab initio calculations reveals that antisite defects associated with oxygen vacancies are primarily present in the SrTiO3 film (STO-f) close to the p-type interface (STO-f/LaAlO3), while oxygen vacancies prevail close to the top n-type interface (LaAlO3/STO-f). At the same interface, misfit dislocations relax the tensile strain of the top LaAlO3 layer. Combining x-ray absorption spectroscopy, x-ray linear dichroism, resonant photoemission spectroscopy, and electron energy loss spectroscopy, we observe that the 3d orbital reconstruction at the interface between LaAlO3 and the SrTiO3 substrate is confined over a few interfacial Ti planes while, at the top n-type interface (LaAlO3/STO-f), the absence of a dichroic signal can be related to the blurring of the interfacial orbital reconstruction due to the heterogeneity of defects.

Abstract licence: CC BY

Reads

Read by people on this page

None yet.

Checked or read by AI through naulon

None yet.

A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.

Are you an author?

Is this your paper?

Claim it to add your note and be paid when agents cite it. Free.