Improved room-temperature-selectivity between Nd and Fe in Nd recovery from Nd-Fe-B magnet

Y. Kataoka, T. Ono, M. Tsubota and 1 more

AIP Advances · 2015

doi:10.1063/1.4935570 (opens in a new tab)

We email you when a new notice or a question about this paper appears.

Abstract

The sustainable society requires the recycling of rare metals. Rare earth Nd is one of rare metals, accompanying huge consumption especially in Nd-Fe-B magnets. Although the wet process using acid is in practical use in the in-plant recycle of sludge, higher selectivity between Nd and Fe at room temperature is desired. We have proposed a pretreatment of corrosion before the dissolution into HCl and the oxalic acid precipitation. The corrosion produces γ-FeOOH and a Nd hydroxide, which have high selectivity for HCl solution at room temperature. Nd can be recovered as Mn2O3-type Nd2O3. The estimated recovery-ratio of Nd reaches to 97%.

Abstract licence: CC BY

Reads

Read by people on this page

None yet.

Checked or read by AI through naulon

None yet.

A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.

Are you an author?

Is this your paper?

Claim it to add your note and be paid when agents cite it. Free.