Effect of High-Temperature Quenching on the Phase Composition, Structure, and Wear Resistance of Ni-Hard Chromium-Nickel Cast Iron

Filippov M.A., Sharapova V.A., Moshechkova L.A. and 1 more

MATEC Web of Conferences · 2021

doi:10.1051/matecconf/202134602025 (opens in a new tab)

We email you when a new notice or a question about this paper appears.

Abstract

Metallographic, micro-X-ray spectral and X-ray structural analyses have been carried out. The quenching temperature increase from 900 to 1150 °C leads to high abrasive wear resistance in Ni-hard chromium-nickel cast iron. The initial hardness decreased before the test from 60 to 35 HRC due to the fact that the phase composition of the metal base before the wear test changes during quenching from medium-carbon martensite with secondary cementite to retained metastable austenite. It contributes to increase the crack resistance of cast iron. Austenite turns into dispersed friction martensite on the working surface in the process of wear testing or operation, as a result of the impact of abrasive particles. This martensite together with a part of cementite provides a high level of hardening and operability of the cast iron secondary microstructure.

Abstract licence: CC BY

Reads

Read by people on this page

None yet.

Checked or read by AI through naulon

None yet.

A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.

Are you an author?

Is this your paper?

Claim it to add your note and be paid when agents cite it. Free.