Role of total reactive oxide ratios on strength development in activated fly ash
Bhagath Singh G.V.P., Subramaniam Kolluru V.L.
MATEC Web of Conferences · 2017
doi:10.1051/matecconf/201712002014 (opens in a new tab)
We email you when a new notice or a question about this paper appears.
Abstract
The role of individual reactive components and process variables such as molarity and temperature on alkaline activation of different low-calcium fly ash is explored. The oxide ratios in the activated system, based on the total silica (total SiO2) in the system consisting of the reactive silica contributed by fly ash and the reactive alumina in fly ash are shown to provide consistent results for achieving the highest strength. For a given total SiO2 content in the system, an increase in the sodium content above a certain dosage does not influence the ultimate compressive strength. An optimum (total SiO2) to Na2O ratio, equal to 2.66 is established for achieving maximum strength. The role of temperature within the range of 60°C-85°C is not significant when the molarity of NaOH is high. A N-A-S-H type gel with Si/Al ratio ranging between 2.5 to 3.0 and the Al/Na ratio varying between 1.30 to 0.9 is formed on decreasing the (total SiO2)/Na2O ratio from 6.55 to 2.66
Abstract licence: CC BY
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.