Experimental research on mechanical properties of high voltage transmission lines after the simulated wildfires
Wang Tianzheng, Tang Zhen, Wang Xinwei and 5 more
MATEC Web of Conferences · 2015
doi:10.1051/matecconf/20153406003 (opens in a new tab)
We email you when a new notice or a question about this paper appears.
Abstract
In order to determine whether the mechanical performance after the fires of high voltage transmission lines meets the requirements of normal use, this article simulates the wildfire, and does the mechanical performance experiment of high voltage transmission lines(HVT lines) after the simulated wildfires. The experiment studied the breaking force and elongation of each layer of 500kv HVT lines after the simulated wildfire. Experimental results show that, after fires, each layer of single aluminum wires of 500kv HVT lines have low breaking force which can be decreased obviously to half of that of new lines. For the steel core, decrease of breaking force is not obvious than aluminum wires, and with the increasing degree of wildfires, it increases gradually to a maximum of 35% of new steel lines’ breaking force. After wildfires, aluminum lines’ resistance ability of deformation decreases significantly, and its plastic deformation increases obviously during uniaxial tension. The steel core has little plastic deformation, and layers of aluminum become fluffy after fires. Therefore, the steel core main bearing load after wildfires.
Abstract licence: CC BY
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.