Effect of sintering temperature on the microstructure and mechanical behavior of porous ceramics made from clay and banana peel powder

M. Mouiya, A. Bouazizi, A. Abourriche and 8 more

Results in Materials · 2019

doi:10.1016/j.rinma.2019.100028 (opens in a new tab)

We email you when a new notice or a question about this paper appears.

Abstract

Porous ceramics were prepared by a solid state process from a mixture of clay and 20 ​wt% banana peels (BPs). BPs were used as an eco-friendly pore-forming agent. Compacted pellets of the dry mixture were calcined at three sintering temperatures, 900, 1000, and 1100 ​°C, for 2 ​h. The effect of sintering temperature on the ceramic properties, such as apparent porosity and mechanical strength, was examined, and an increase in the sintering temperature from 900 to 1100 ​°C yielded porous ceramics with decreased porosity and increased mechanical strength. To obtain porous ceramics (40.2 ​vol% porosity) with sufficient indirect tensile strength (8 ​MPa), the optimum sintering temperature was determined to be 1100 ​°C.

Abstract licence: CC BY-NC

Reads

Read by people on this page

None yet.

Checked or read by AI through naulon

None yet.

A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.

Are you an author?

Is this your paper?

Claim it to add your note and be paid when agents cite it. Free.