Combinatorial design of amorphous TaNiSiC thin films with enhanced hardness, thermal stability, and corrosion resistance
Maciej Kaplan, Aishwarya Srinath, Lars Riekehr and 3 more
Materials & Design · 2022
doi:10.1016/j.matdes.2022.110827 (opens in a new tab)
We email you when a new notice or a question about this paper appears.
Abstract
Amorphous TaNiSiC and TaNiC films (with varying Ta/Ni and Si/C ratios) were deposited using combinatorial magnetron sputtering. The TaNiSiC films remained X-ray amorphous after four hour-long annealings up to 700 °C, while TaNiC alloys with high Ni and C contents crystallized. These differences were attributed to a strong driving force for separation of Ni and C in TaNiC, whereas the addition of Si, due to its solubility in the other elements, reduced the elemental segregation in TaNiSiC. The as-deposited TaNiSiC films exhibited hardnesses of 9–12 GPa. Annealing led to an increase in hardness by 2–4 GPa, due to decreases in average atomic distance, as evidenced by X-ray diffraction measurements. Potentiodynamic polarizations from –0.7 to +1.5 V vs. Ag/AgCl (3 M NaCl) in 10 mM sodium borate showed lower current densities by up to 2 orders of magnitude with increasing Ta content (28–52 at.%). Changes in Si/C content (7–13 at.% Si) had no effect. However, optical microscopy showed that TaNiSiC films with high Si/low C contents (13/10 at.%) suffered much less localized etching compared to TaNiC films. Thus, Si had a significant role in increasing the mechanical strength, corrosion resistance, and thermal stability of the TaNiSiC films.
Abstract licence: CC BY-NC
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.