On the fracture behavior of Cr2AlC coatings
B. Völker, B. Stelzer, S. Mráz and 5 more
Materials & Design · 2021
doi:10.1016/j.matdes.2021.109757 (opens in a new tab)
We email you when a new notice or a question about this paper appears.
Abstract
Bulk MAX phase materials were investigated heavily in the last decades due to their advantageous combination of metallic and ceramic properties. In recent years, MAX phases also gained the interest of the protective coatings community. Cr2AlC is a very promising material, since the crystalline MAX phase can be deposited at comparatively low (550 °C) substrate temperatures. Another advantage of the Cr2AlC MAX phase is its self-healing ability. The goal of this investigation was to characterize the fracture toughness of Cr2AlC protective coatings using in situ SEM micro-cantilever tests and to determine the influence of different microstructures on the fracture behavior. Surprisingly, the fracture toughness is only moderately affected by the microstructure of the crystalline samples investigated here, which reveal a fracture toughness ranging from 1.8 ± 0.1 MPam1/2 to 2.4 ± 0.2 MPam1/2.In contrast to that, it could be shown that there is a significant increase in fracture toughness for the amorphous coating with identical chemical composition (4.1 ± 0.5 MPam1/2) of almost twice the fracture toughness compared to the crystalline coatings. The detrimental influence of grain boundaries in the crystalline coating and the lack of grain boundaries in the amorphous sample might explain the formidable fracture toughness.
Abstract licence: CC BY-NC
Reads
Read by people on this page
None yet.
Checked or read by AI through naulon
None yet.
A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.
Are you an author?
Is this your paper?
Claim it to add your note and be paid when agents cite it. Free.