Complete chemical and structural characterization of selenium-incorporated hydroxyapatite

Baris Alkan, Caner Durucan

Journal of Materials Science: Materials in Medicine · 2021

doi:10.1007/s10856-021-06631-6 (opens in a new tab)

We email you when a new notice or a question about this paper appears.

Abstract

Hydroxyapatite (HAp) has long been used as synthetic bone tissue replacement material. Recent advances in this area have led to development of dual-functional bioceramics exhibiting high biocompability/osteoconductivity together with the therapeutic effect. Selenium, in that respect, is an effective therapeutic agent with promising antioxidant activity and anticancer effects. In this study, selenium-incorporated hydroxyapatite (HAp:Se) particles have been synthesized by modified aqueous precipitation method using calcium (Ca(NO 3 ) 2 ·4H 2 O) and phosphate ((NH 4 ) 2 HPO 4 ) salts and sodium selenite (Na 2 SeO 3 ). The effects of selenium incorporation and post-synthesis calcination treatment (900–1100 °C) on physical, chemical properties and crystal structure of resultant HAp powders have been investigated. Complete chemical identification was performed with spectroscopical analyses including Fourier transform infrared and x-ray photoelectron spectroscopy to elucidate the mechanism and chemical nature of selenium incorporation in HAp. Meanwhile, detailed x-ray diffraction studies by Rietveld refinement have conducted to explain changes in the HAp crystal structure upon selenium incorporation.

Abstract licence: CC BY-NC-ND

Reads

Read by people on this page

None yet.

Checked or read by AI through naulon

None yet.

A person counts once a day per paper. We keep no cookie and no address: a reader is a hash that changes every day. Any month under five reads shows no number.

Are you an author?

Is this your paper?

Claim it to add your note and be paid when agents cite it. Free.